Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.2 MPa | 3950 psi | 2 in/min; ASTM D638 |
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 27.2 MPa | 3940 psi | AVG; ASTM D412 Method A |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 27.2 MPa | 3940 psi | AVG; ASTM D412 Method A |
Seals Eastern 7345 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 27.2 MPa | 3950 psi | ASTM D638 |
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Tensile Strength at Break | 27.2 MPa | 3950 psi | ASTM D638 Die C |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |