Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 16.7 MPa | 2420 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Tensile Strength at Break | 16.7 MPa | 2420 psi | 5mm/min; ASTM D638 |
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade
(discontinued **) TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Tensile Strength at Break | 16.7 MPa @Temperature 145 °C, Time 2100 sec |
2420 psi @Temperature 293 °F, Time 0.583 hour |
cured; ASTM D412 |
LG Chemical BR 1208 Polybutadiene Polymer Description: BR1208 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process employing a stereospecific catalyst to control microstructure, molecular weight and molecular.. |
|||
Tensile Strength at Break | 16.7 MPa @Temperature 145 °C, Time 2100 sec |
2420 psi @Temperature 293 °F, Time 0.583 hour |
cured; ASTM D412 |
LG Chemical BR 1280 Polybutadiene Polymer BR 1280 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process polymerization process employing a stereospecific catalyst to control microstructure, molecular weight an.. |
|||
Tensile Strength at Break | 16.7 MPa | 2420 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HI1100 High density polyethylene HI1100 is a non UV stabilised high density polyethylene for injection molding. HI1100 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 .. |
|||
Tensile Strength at Break | 16.7 MPa | 2420 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap.. |
|||
Tensile Strength at Break | 16.7 MPa | 2420 psi | ASTM D638 |
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified .. |
|||
Tensile Strength at Break | 16.7 MPa | 2420 psi | ASTM D412 |
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |