Mechanical Properties Metric English Comments
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D638
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film
The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This..
Tensile Strength at Break 13.5 MPa

@Temperature 110 °C,
Time 1.21e+6 sec
1960 psi

@Temperature 230 °F,
Time 336 hour
500mm/min; ASTM D638
LG Chemical LUTENE CCO550BK PE Compound
Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo..
Tensile Strength at Break 13.5 MPa
1960 psi
ISO R 527
Stir SpA SG 55 ATC (PVC)
Application: Extrusion non-toxic seal for wood window and door framesInformation provided by STIR SpA
Tensile Strength at Break 13.5 MPa
1960 psi
ISO R 527
Stir SpA SR 70 (PVC)
Application: Extrusion sheath with good flexibility type TM-2Cold flex = -33°CInformation provided by STIR SpA
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D412
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Tensile Strength at Break >= 13.5 MPa
>= 1960 psi
after aging (168h, 136°C); ASTM D638
Borealis LR4201R Polyethylene Insulation Compound, Crosslinkable
LR4201R is a natural low-density crosslinkable polyethylene compound. Applications: LR4201R is intended for insulation of XLPE power cables with rated voltages up to 72 kV. Specifications: ISO 1872..
Tensile Strength at Break 13.5 MPa
1960 psi
after crosslinking process; IEC 60811
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC
This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende..
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D3759
3M 483 Polyethylene Tape
3M™ Polyethylene Tape 483 has a polyethylene backing with a rubber adhesive for many general purpose applications including sealing, color coding, protecting, moisture proofing. Black tape has exce..
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D638
IRPC Polimaxx Polene V1160 High Density Polyethylene
CHARACTERISTICS: GOOD FLOWABILITYAPPLICATIONS: INJECTION MOLDING FOR LIGHT WEIGHT HOUSEHOLDS, TOYS, FOOD CONTAINERS, COSMETICS CLOSURES, DISPOSABLE ARTICLES, LARGE MOLDING AND COMPLICATED PARTS