Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.1 MPa | 1750 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 60ANS200 Thermoplastic Elastomer
(discontinued **) A soft, translucent thermoplastic elastomer (TPE) with a relative haze of 85 to 90%. This material is shear-dependent and can be processed on conventional thermoplastics equipment for injection mold.. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D638 |
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w.. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D412 |
DuPont Elvax® 40L-03 Strippable Semiconductive Insulation Shield Formulation
(discontinued **) Elvax® 40L-03 strippable semiconductive insulation shield.Information provided by DuPont. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D412 |
DuPont Elvax® 40L-08 Strippable Semiconductive Insulation Shield Formulation
(discontinued **) Elvax® 40L-08 strippable semiconductive insulation shield.Information provided by DuPont. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | Type IV specimen; ASTM D638 |
LyondellBasell Petrothene® NA216000 Low Density Polyethylene ApplicationsPETROTHENE NA 216-000 is a general purpose, heavy and medium weight coating resin, capable of coating weights down to 7.0 lbs/ream at line speeds of 1200 ft/min. It can be applied to pa.. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C).. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 550 Perfluoroelastomer Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in d.. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 - 13.8 MPa | 1750 - 2000 psi | |
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ISO R 527 |
Stir SpA AF 77 CZ (PVC) Application: Extrusion flame resistant sheath CEI 20-11 type TM 2Information provided by STIR SpA |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D638 |
Teknor Apex APEX® 90-A471R-6-NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno.. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D412 |
Teknor Apex Monprene® MP 1097F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D412 |
Teknor Apex Telcar® TL-81-D965-P Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | ASTM D412 |
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 12.1 MPa | 1760 psi | ASTM D412 |
Teknor Apex APEX® 3075-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | Forming |
LG Chemical NBR 8300 High Acrylonitrile Polymer Description: NBR 8300 is a copolymer of butadiene-acrylonitrile and the powdered nitrile elastomer manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 8300 has .. |
|||
Tensile Strength at Break | 12.1 MPa | 1750 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2161X Fluoroelastomer
(discontinued **) Composition: di-polymer of vinylidene fluoride and hexafluoropropyleneMedium viscosityProcess targets: compression and transfer molding, and calenderingProprietary incorporated cure technologyExcell.. |