Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Tensile Strength at Break | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT226 Thermoplastic Elastomer (TPE) Versaflex™ HC MT226 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT226 has been specially formulated to be free of any plasticizers . .. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ISO 527 |
Polimeri Europa Riblene® GP 26 Low Density Polyethylene - Coating Grade Riblene GP 26 is a high fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GP 26 is suitable for coating applications where low neck-in and high draw-down are key factors. F.. |
|||
Tensile Strength at Break | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
SABIC HP7022 Low Density Polyethylene for Injection Molding Product Description: HP7022 is a Low Density Polyethylene offering a unique combination of consistent processability, flexibility and toughness. Articles manufactured from HP7022 exhibit excellent.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
LyondellBasell Microthene® G MN71020 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
LyondellBasell Microthene® G MN72700 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D412 |
Teknor Apex Monprene® MP-1698 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D412 |
Teknor Apex Monprene® MP-1766-R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D412 |
Teknor Apex Monprene® MP 1225B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D412 |
Teknor Apex Telcar® TL-2454A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
Borealis LE0315 Polyethylene Compound, Crosslinkable, Semiconductive LE0315 is an Easy Strippable Semi conductive Insulation Shield for EPR Insulated, Medium Voltage (5-46 kV) Cables. Strip forces range from 5 to 10 lbs/0.5". Specifications: LE0315 meets the applica.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | 500mm/min; ASTM D638 Type IV Specimen |
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
Teknor Apex Vidux® 100-1A Polyvinyl Chloride, Flexible Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ISO R 527 |
Fainplast Compounds GS 0145/R Flexible PVC, Injection Molding, Lead Free Technical items with rubber/PU |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ISO R 527 |
Fainplast Compounds GS 64 Flexible PVC, Injection Molding for Footwear Soles |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ISO R 527 |
Fainplast Compounds GS 64/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ISO R 527 |
Fainplast Compounds GSK 78 Flexible PVC, Injection Molding, Lead Free Plugs |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ISO R 527 |
Fainplast Compounds PM 55 Flexible PVC, Lead Free Gaskets for frames |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | 25mm/min; ISO 527 |
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage.. |
|||
Tensile Strength at Break | 11.0 MPa | 1600 psi | |
Master Bond UV15X-6NONMED-2 Abrasion Resistant UV Curable Compound Description: Master Bond Polymer System UV15X-6NONMED-2 is a newly developed one component clear, non-yellowing, UV curable urethane elastomer system possessing high flexibility and abrasion resista.. |