Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.01 - 16.0 J/cm | 15.0 - 30.0 ft-lb/in | Average value: 10.9 J/cm Grade Count:3 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Unnotched | 5.34 - 16.0 J/cm | 10.0 - 30.0 ft-lb/in | Average value: 8.90 J/cm Grade Count:3 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Izod Impact, Unnotched | 2.67 - 16.0 J/cm | 5.00 - 30.0 ft-lb/in | Average value: 5.32 J/cm Grade Count:64 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched | 2.14 - 16.0 J/cm | 4.00 - 30.0 ft-lb/in | Average value: 8.37 J/cm Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched | 1.23 - 16.0 J/cm | 2.30 - 30.0 ft-lb/in | Average value: 11.1 J/cm Grade Count:51 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Unnotched | 5.34 - 16.0 J/cm | 10.0 - 30.0 ft-lb/in | Average value: 9.65 J/cm Grade Count:13 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Unnotched | 0.801 - 16.0 J/cm | 1.50 - 30.0 ft-lb/in | Average value: 7.99 J/cm Grade Count:66 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Unnotched | 2.40 - 16.0 J/cm | 4.50 - 30.0 ft-lb/in | Average value: 6.99 J/cm Grade Count:10 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Izod Impact, Unnotched | 4.27 - 16.0 J/cm | 8.00 - 30.0 ft-lb/in | Average value: 10.5 J/cm Grade Count:7 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Izod Impact, Unnotched | 3.74 - 16.0 J/cm | 7.00 - 30.0 ft-lb/in | Average value: 9.28 J/cm Grade Count:13 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |