Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.60 - 6.94 J/cm
3.00 - 13.0 ft-lb/in
Average value: 3.72 J/cm Grade Count:36
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched 3.74 - 6.94 J/cm
7.00 - 13.0 ft-lb/in
Average value: 5.31 J/cm Grade Count:19
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched 4.27 - 6.94 J/cm
8.00 - 13.0 ft-lb/in
Average value: 6.10 J/cm Grade Count:5
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Unnotched 4.81 - 6.94 J/cm
9.00 - 13.0 ft-lb/in
Average value: 5.61 J/cm Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Izod Impact, Unnotched 1.07 - 6.94 J/cm
2.00 - 13.0 ft-lb/in
Average value: 3.89 J/cm Grade Count:35
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Izod Impact, Unnotched 3.74 - 6.94 J/cm
7.00 - 13.0 ft-lb/in
Average value: 5.15 J/cm Grade Count:24
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Izod Impact, Unnotched 3.35 - 6.94 J/cm
6.28 - 13.0 ft-lb/in
Average value: 5.18 J/cm Grade Count:9
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Izod Impact, Unnotched 3.74 - 6.94 J/cm
7.00 - 13.0 ft-lb/in
Average value: 4.68 J/cm Grade Count:19
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..