Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.07 J/cm | 9.50 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LCF30-PES Polyethersulfone, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyethersulfone with 30% long carbon fiber reinforcementInformation provided by Plast.. |
|||
Izod Impact, Unnotched | 5.07 J/cm @Temperature 23.0 °C |
9.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Unnotched | 5.07 J/cm @Temperature 23.0 °C |
9.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copolymer LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Unnotched | 5.07 J/cm | 9.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Unnotched | 5.07 J/cm | 9.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Unnotched | 5.07 J/cm | 9.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1510 compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Unnotched | 5.07 J/cm @Thickness 3.17 mm |
9.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS WM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 5.07 J/cm @Thickness 3.17 mm |
9.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PBT/ABS GF/M40 FR 40/40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Fiber Reinforcement, 40/40% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 5.07 J/cm | 9.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.07 J/cm @Thickness 3.17 mm |
9.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
Izod Impact, Unnotched | 5.07 J/cm | 9.50 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |