Polymer Property : Izod Impact, Unnotched = 9.46 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.05 J/cm

@Temperature 23.0 °C
9.46 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp GFL14 PSU
LNP* Lubricomp* GFL14 is a compound based on Polysulfone containing Glass Fiber and PTFE Lubricant.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 5.05 J/cm
9.46 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX99620C PC
LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Izod Impact, Unnotched 5.05 J/cm
9.46 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES
LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible.
Izod Impact, Unnotched 5.05 J/cm
9.46 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON FX91304 PE
LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Izod Impact, Unnotched 5.05 J/cm
9.46 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..