Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.52 J/cm @Thickness 3.18 mm |
6.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Izod Impact, Unnotched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Unnotched | 3.52 J/cm @Temperature 23.0 °C |
6.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Izod Impact, Unnotched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 109 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |