Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.17 J/cm | 5.94 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
Izod Impact, Unnotched | 3.17 J/cm | 5.94 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 3.17 J/cm @Temperature 23.0 °C |
5.94 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp 4X08423 LNP* Thermocomp* 4X08423 is a compound based on Perfluoroalkoxy Polymer (PFA) containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 3.17 J/cm | 5.94 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |