Polymer Property : Izod Impact, Unnotched = 3.99 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.13 J/cm

@Temperature 23.0 °C
3.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66
LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f..
Izod Impact, Unnotched 2.13 J/cm
3.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66
LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 2.13 J/cm
3.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific)
LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 2.13 J/cm
3.99 ft-lb/in
ASTM D256
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer
40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..
Izod Impact, Unnotched 2.13 J/cm
3.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON ME006 PP (Asia Pacific)
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.