Mechanical Properties Metric English Comments
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D-4812
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.17 mm
24.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PEI BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.17 mm
24.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PEI HF BK
Availability: North AmericaForms: PelletsFeatures: High FlowAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.17 mm
24.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PEI TX5 LE
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Low Extractables and LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.17 mm
24.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PEI/C GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 12.8 J/cm

@Thickness 3.17 mm
24.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 GF40 TL10 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat StabilizedInformation p..
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66
LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized.
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® RMC-20 20% Calcium Carbonate-Reinforced Polypropylene, High Impact
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin..
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized
Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar..
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D256A
Total PPH 3429 Polypropylene, Injection Molding Grade
LTHA injection molding homopolymerLTHA - FINA 3429 is engineered with an LTHA additive system that gives excellent leach resistance in hot/wet environments that contain bleach and laundry detergents..
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo..