Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.7 - 5340 J/cm | 22.0 - 10000 ft-lb/in | Average value: 13.4 J/cm Grade Count:7 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 11.7 J/cm @Thickness 3.17 mm |
22.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 11.7 J/cm @Thickness 3.17 mm |
22.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D4812 |
Teknor Apex Terraloy™ BP 13000A Thermoplastic Starch + PP Notes: Terraloy™ BP-13000A is a Thermoplastic Starch/PP ready-to-process compound that contains up to 30% of TPS renewable content. This compound is intended for injection molding as well as extru.. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Adell ZS-10 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Adell ZS-30 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade BRC R7560 CLR 221 is a food grade PVC bottle compound made with 100% FDA approved ingredients. This product exhibits excellent clarity and can be used in many applications where food contact is req.. |