Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.68 J/cm | 12.5 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LCF10/LGF30 - PP Polypropylene, 40% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66 LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Izod Impact, Unnotched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Izod Impact, Unnotched | 6.69 J/cm | 12.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Izod Impact, Unnotched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber. |
|||
Izod Impact, Unnotched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 (Asia Pacific) LNP* Thermocomp* RFB66 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. |
|||
Izod Impact, Unnotched | 6.67 J/cm | 12.5 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® RMT-20V 20% Talc-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMT-V series compounds are high impact, UV stabilized polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and the abili.. |
|||
Izod Impact, Unnotched | 6.67 - 5340 J/cm | 12.5 - 10000 ft-lb/in | Average value: 9.98 J/cm Grade Count:6 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |