Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.41 - 5340 J/cm | 12.0 - 10000 ft-lb/in | Average value: 12.8 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated. |
|||
Izod Impact, Unnotched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA6/6 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Izod Impact, Unnotched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp JX89569 PES LNP THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 6.40 J/cm @Thickness 3.18 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Izod Impact, Unnotched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific) LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |