Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ABL12 ABS LNP* Lubricomp* ABL12 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Glass Bead and 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.59 J/cm @Temperature 23.0 °C |
10.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12 LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Unnotched | 5.63 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.58 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC (Asia Pacific) LNP* THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing Glass Fiber, Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 (Asia Pacific) LNP* Thermocomp* RF0069SZ is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-16769N Internally Lubricated, Glass Fiber Reinforced PPS Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 632 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |