Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.720 J/cm | 1.35 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AFB42 ABS LNP* THERMOCOMP* AFB42 is a compound based on ABS containing 10% Glass Fiber, 20% Glass Bead. |
|||
Izod Impact, Unnotched | 0.721 J/cm | 1.35 ft-lb/in | |
Trelleborg AEM Syntac® Eccolite® Ultra Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robus.. |
|||
Izod Impact, Unnotched | 0.720 J/cm | 1.35 ft-lb/in | |
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam Eccolite Ultra syntactic foam plug assist materials a new engineered thermoplastic compound incorporating Eccospheres, glass microspheres. It is one of the toughest materials designed for the therm.. |