Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.23 J/cm | 17.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 9.23 J/cm | 17.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 9.23 J/cm | 17.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched | 9.23 J/cm @Temperature 23.0 °C |
17.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 9.23 J/cm | 17.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |