Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.93 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched | 7.93 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific) LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 7.93 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |