Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontinued **)< Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Izod Impact, Unnotched | 6.41 J/cm - NB | 12.0 ft-lb/in - NB | Average value: 6.41 J/cm Grade Count:3 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 CF33 ML2 BK 33% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 33% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceAp.. |
|||
Izod Impact, Unnotched | 6.41 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 624 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.43% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 6.41 - 8.54 J/cm | 12.0 - 16.0 ft-lb/in | Average value: 7.35 J/cm Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |