Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP AL001 ABS LNP LUBRICOMP* AL-4010 HP is a compound based on Acrylonitrile Butadiene Styrene resin containing 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of .. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Izod Impact, Unnotched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro.. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IF006L PA 6/12 (Asia Pacific) LNP* THERMOCOMP* IF006L is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RX02743 PA 66 LNP* Thermocomp* RX02743 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66 LNP THERMOCOMP* RW004 is a compound based on Nylon 66 resin containing Wollastonite. |
|||
Izod Impact, Unnotched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |