Polymer Property : Izod Impact, Unnotched = 4.90 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE0029 PC
LNP* STAT-KON* DE0029 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific)
LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE004 PC
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Izod Impact, Unnotched 4.90 J/cm

@Temperature -30.0 °C
9.18 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No..
Izod Impact, Unnotched 4.90 J/cm

@Temperature -30.0 °C
9.18 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No..
Izod Impact, Unnotched 4.90 J/cm
9.18 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Izod Impact, Unnotched 4.90 J/cm

@Temperature -30.0 °C
9.18 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..