Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.41 J/cm | 8.26 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific) LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 4.41 J/cm | 8.26 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Izod Impact, Unnotched | 4.41 J/cm @Temperature 23.0 °C |
8.26 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |
|||
Izod Impact, Unnotched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Izod Impact, Unnotched | 4.41 J/cm @Thickness 3.17 mm |
8.27 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Izod Impact, Unnotched | 4.41 J/cm | 8.26 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 (Asia Pacific) LNP* Thermocomp* RFB53XXZ is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. |