Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.05 J/cm | 7.59 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Izod Impact, Unnotched | 4.05 J/cm | 7.59 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.05 J/cm | 7.59 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS - Branched LNP* THERMOCOMP* OF006A is a compound based on PPS - Branched resin containing 30% Glass Fiber. |