Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 133 PC Nonhalogenated. 3.5 MFR. UV-stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 141R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® I2220 PC General purpose polycarbonate with melt flow rate of 10.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® PPC4701 PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® PPC4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® VR2520 PC General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 943 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 950A PC (Asia Pacific) Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific) Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® FXD941A PC FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Co.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature -30.0 °C |
60.02 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |