Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.60 J/cm | 4.87 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Izod Impact, Unnotched | 2.60 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
4.87 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **) PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Izod Impact, Unnotched | 2.60 J/cm | 4.87 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Izod Impact, Unnotched | 2.60 J/cm | 4.87 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Izod Impact, Unnotched | 2.60 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
4.87 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **) PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te.. |