Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.14 - 7.47 J/cm | 4.00 - 14.0 ft-lb/in | Average value: 3.36 J/cm Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Izod Impact, Unnotched | 2.14 - 5.34 J/cm | 4.00 - 10.0 ft-lb/in | Average value: 3.01 J/cm Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched | 2.14 - 16.0 J/cm | 4.00 - 30.0 ft-lb/in | Average value: 8.37 J/cm Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched | 2.14 - 5340 J/cm | 4.00 - 10000 ft-lb/in | Average value: 3.99 J/cm Grade Count:6 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Unnotched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HIPS GF50 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P-40TC-5100 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | Average value: 2.76 J/cm Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |