Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.03 J/cm | 3.80 ft-lb/in | |
Reliance Industries Polypropylene - Suzorite mica (untreated) filler Information provided by Reliance Industries |
|||
Izod Impact, Unnotched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Temperature -40.0 °C |
3.80 ft-lb/in @Temperature -40.0 °F |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GB30 FR 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearance: BlackTPCI# .. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GB20 L 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GB10 L 10% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GB15 15% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GB30 L 30% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PPS/F GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackIn.. |
|||
Izod Impact, Unnotched | 2.03 J/cm @Thickness 3.18 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |