Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D4812
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
Malvern Minerals Nylon with Novacite® L-337 Quartz Filler
Product data demonstrates the effect of the Novacite® (untreated lamellar quartz) filler. A separate entry demonstrates the effect of treated Novakup® filler in nylon. The specific nylon use..
Izod Impact, Unnotched 1.92 J/cm

@Temperature 23.0 °C
3.60 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp OP005XXC PPS
LNP LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-..
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS - LINEAR
LNP LUBRICOMP* OP005XXC is a compound based on PPS - Linear resin containing 25% PTFE/Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS (Asia Pacific)
LNP* LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D256
Spartech Weather-Pro G Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS
LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing.