Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256 |
Hyosung Topilene J340F PP J340F Film Grade Impact CopolymerApplications: Retort CPPCharacteristics:ProcessabilityHigh impactInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256 |
Hyosung Topilene J351F PP J351F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Izod Impact, Unnotched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Izod Impact, Unnotched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Izod Impact, Unnotched | 0.883 - 9.60 J/cm | 1.65 - 18.0 ft-lb/in | Average value: 5.64 J/cm Grade Count:10 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |