Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 120 MPa @Strain 3.50 % |
17400 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Yield Strength | 120 MPa @Strain 3.50 % |
17400 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |