Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² @Temperature 23.0 °C |
1.90 - 2.86 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Charpy Impact Unnotched | 0.500 - 0.600 J/cm² | 2.38 - 2.86 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² @Temperature 23.0 °C |
1.90 - 2.86 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | ISO 179 |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |