Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.00 - 2.50 J/cm² @Temperature -30.0 - -30.0 °C |
9.52 - 11.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.25 J/cm² Grade Count:2 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Charpy Impact Unnotched | 1.30 - 2.50 J/cm² | 6.19 - 11.9 ft-lb/in² | Average value: 1.65 J/cm² Grade Count:15 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact Unnotched | 0.400 - 2.50 J/cm² | 1.90 - 11.9 ft-lb/in² | Average value: 1.38 J/cm² Grade Count:4 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Charpy Impact Unnotched | 1.00 - 2.50 J/cm² @Temperature -30.0 - -20.0 °C |
4.76 - 11.9 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 2.00 J/cm² Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Charpy Impact Unnotched | 2.50 - 2.50 J/cm² @Temperature -20.0 - -20.0 °C |
11.9 - 11.9 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 2.50 J/cm² Grade Count:1 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 2.50 - 2.50 J/cm² @Temperature -20.0 - -20.0 °C |
11.9 - 11.9 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 2.50 J/cm² Grade Count:2 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Charpy Impact Unnotched | 2.00 - 2.50 J/cm² @Temperature -20.0 - -20.0 °C |
9.52 - 11.9 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 2.25 J/cm² Grade Count:2 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Charpy Impact Unnotched | 1.00 - 2.50 J/cm² | 4.76 - 11.9 ft-lb/in² | Average value: 1.70 J/cm² Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Charpy Impact Unnotched | 1.50 - 2.50 J/cm² @Temperature -30.0 - 5.00 °C |
7.14 - 11.9 ft-lb/in² @Temperature -22.0 - 41.0 °F |
Average value: 2.00 J/cm² Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |