Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.30 - 1000 J/cm² | 30.0 - 4760 ft-lb/in² | Average value: 12.6 J/cm² Grade Count:18 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² | 30.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² | 30.0 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² @Temperature -30.0 °C |
30.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² | 30.0 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² | 30.0 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² @Temperature 23.0 °C |
30.0 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Akulon® SG-KGS6 PA66-GF30 FR 30% Glass Reinforced, Halogen free and free of red phosphorous |
|||
Charpy Impact Unnotched | 6.30 J/cm² | 30.0 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |