Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.30 J/cm² | 25.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.30 J/cm² @Temperature -40.0 °C |
25.2 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 HS-SG-GV2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.30 J/cm² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 5.30 J/cm² @Temperature -40.0 °C |
25.2 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 HS-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.30 J/cm² | 25.2 ft-lb/in² | ISO 179/1eU |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact Unnotched | 5.30 J/cm² | 25.2 ft-lb/in² | EN ISO 179/1eU |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Charpy Impact Unnotched | 5.30 J/cm² | 25.2 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Charpy Impact Unnotched | 5.30 J/cm² @Temperature -30.0 °C |
25.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |