Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 45.0 J/cm² | 214 ft-lb/in² | partial break; ISO 179-1/1eU |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
Charpy Impact Unnotched | 45.0 J/cm² @Temperature -30.0 °C |
214 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |