Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.40 J/cm² @Temperature -30.0 °C |
20.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.40 J/cm² @Temperature 23.0 °C |
20.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact Unnotched | 4.40 J/cm² - NB @Temperature -40.0 - -20.0 °C |
20.9 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 8.98 J/cm² Grade Count:68 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² @Temperature 23.0 °C |
20.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eU |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/BK PBT, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² @Temperature -20.0 °C |
20.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² @Temperature -30.0 °C |
20.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | ISO 179 |
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co.. |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.40 J/cm² | 20.9 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |