Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² @Temperature 23.0 °C |
0.952 - 1.43 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact Unnotched | 0.200 - 0.400 J/cm² | 0.952 - 1.90 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179/1eU |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179/1eU |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact Unnotched | 0.200 - 1.50 J/cm² | 0.952 - 7.14 ft-lb/in² | Average value: 0.730 J/cm² Grade Count:9 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Charpy Impact Unnotched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Stanyl® TC155 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Charpy Impact Unnotched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Stanyl® TC551 PA46 FR(17) Thermal conductive material, Flame Retardant |
|||
Charpy Impact Unnotched | 0.200 - 0.900 J/cm² | 0.952 - 4.28 ft-lb/in² | Average value: 0.590 J/cm² Grade Count:5 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |