Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.400 - 0.600 J/cm²

@Temperature 23.0 °C
1.90 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eU
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Charpy Impact Unnotched 0.500 - 0.600 J/cm²
2.38 - 2.86 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²

@Temperature 23.0 °C
1.90 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eU
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
ISO 179
Vyncolit X658 Novolac Phenolic