Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 35.0 J/cm² @Temperature 23.0 °C |
167 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Charpy Impact Unnotched | 35.0 J/cm² | 167 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Charpy Impact Unnotched | 35.0 J/cm² | 167 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers with very low .. |
|||
Charpy Impact Unnotched | 35.0 J/cm² | 167 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Charpy Impact Unnotched | 35.0 J/cm² @Temperature -30.0 °C |
167 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
Charpy Impact Unnotched | 35.0 J/cm² @Temperature -40.0 °C |
167 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
Charpy Impact Unnotched | 35.0 J/cm² @Temperature -30.0 °C |
167 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |