Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.850 - 50.0 J/cm² | 4.05 - 238 ft-lb/in² | Average value: 5.67 J/cm² Grade Count:130 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Charpy Impact Unnotched | 0.850 J/cm² @Temperature 23.0 °C |
4.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Charpy Impact Unnotched | 0.850 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4.05 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.850 J/cm² Grade Count:3 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact Unnotched | 0.850 - 1.00 J/cm² | 4.05 - 4.76 ft-lb/in² | ISO 179 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Charpy Impact Unnotched | 0.850 J/cm² | 4.04 ft-lb/in² | ISO 179-1 |
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa.. |
|||
Charpy Impact Unnotched | 0.850 J/cm² @Temperature -30.0 °C |
4.05 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry) Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro.. |
|||
Charpy Impact Unnotched | 0.850 J/cm² @Temperature 23.0 °C |
4.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
Charpy Impact Unnotched | 0.850 J/cm² @Temperature 23.0 °C |
4.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |