Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | 4.5 t | 4.5 t | t ≤ 1.8 mm |
Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed Nominal Composition: Ti-6 Al-4 V Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength .. |
|||
Bend Radius, Minimum | 4.5 t @Thickness 2.00 mm |
4.5 t @Thickness 0.0787 in |
Typical; sheet |
TIMET 8-1-1 Titanium Alloy (Ti-8Al-1Mo-1V); Annealed Sheet Industry Specifications: USA Aerospace: AMS 4915,4916. France: T-A8DV. Features: Designed for creep resistance up to 450°C, used primarily in engine applications such as forged compressor blades.. |
|||
Bend Radius, Minimum | 4.5 t | 4.5 t | Typical; on 0.078 in (2 mm) sheet |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit.. |
|||
Bend Radius, Minimum | 4.5 t @Thickness 2.00 mm |
4.5 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi.. |
|||
Bend Radius, Minimum | 4.5 t | 4.5 t | Typical; on 0.078 in (2 mm) sheet |
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm.. |
|||
Bend Radius, Minimum | 4.5 t @Thickness 2.00 mm |
4.5 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, .. |