Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink F40A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | t = 3.0 mm |
SSAB Tunnplat Docol® 420YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | t = 1.5 mm |
SSAB Tunnplat Docol® 500YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 180 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 220 RP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 220 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 260 RP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 260 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 260YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 280YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 350YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 420YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal 500YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal B420 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal B500 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal F26 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal F30 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal F36 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Dogal F40 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 315MC HSLA Steel HSLA SteelCharacteristics: For hot-dip galvanizing, a thin Zn coating (50-80 microns) is specified.Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better pr.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 355MC HSLA Steel HSLA SteelCharacteristics: For hot-dip galvanizing, a thin Zn coating (50-80 microns) is specified.Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better pr.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 390XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 390YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 420MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 460MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 490XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 0.50 t | >= 0.50 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink F36A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Bend Radius, Minimum | 0.50 t | 0.50 t | ISO 7438 |
ThyssenKrupp PAS 355 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Bend Radius, Minimum | 0.50 t | 0.50 t | ISO 7438 |
ThyssenKrupp PAS 380 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Bend Radius, Minimum | 0.50 t | 0.50 t | ISO 7438 |
ThyssenKrupp PAS 420 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |