Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.0800 J/cm² @Temperature -20.0 °C |
0.381 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i.. |
|||
Charpy Impact, Notched | 0.0800 J/cm² @Temperature -20.0 °C |
0.381 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact, Notched | 0.0800 J/cm² @Temperature -20.0 °C |
0.381 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact, Notched | 0.0800 J/cm² @Temperature -30.0 °C |
0.381 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
Charpy Impact, Notched | 0.0800 J/cm² @Temperature -30.0 °C |
0.381 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |