Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.399 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature 0.000 °C |
1.90 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMN 303 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for high heat ageing resistance for automotive interior trim applications such as instrument panels.Availability: Africa & Mi.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature 0.000 °C |
1.90 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMU 101 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance and good UV resistance are required.Availa.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature 0.000 °C |
1.90 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMU 101D Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance, minimum dust deposit and good UV resistan.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature 0.000 °C |
1.90 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil PP7033L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil PP7085E1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature 0.000 °C |
1.90 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil PPU0009F Polypropylene Impact Copolymer Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobi.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |