Mechanical Properties Metric English Comments
Izod Impact, Notched 1.0678 - 2.1356 J/cm

@Temperature -40.0 - -20.0 °C
2.0004 - 4.0009 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 1.51 J/cm Grade Count:2
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Izod Impact, Notched 1.0678 - 2.1356 J/cm

@Thickness 3.17 - 3.17 mm
2.0004 - 4.0009 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.51 J/cm Grade Count:2
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Izod Impact, Notched 1.0678 - 1.0678 J/cm

@Temperature -40.0 - -40.0 °C
2.0004 - 2.0004 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.05 J/cm Grade Count:9
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched 1.0678 - 1.0678 J/cm

@Thickness 3.17 - 3.17 mm
2.0004 - 2.0004 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.05 J/cm Grade Count:9
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched 1.0678 - 1.0678 J/cm

@Temperature -40.0 - -40.0 °C
2.0004 - 2.0004 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.850 J/cm Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Izod Impact, Notched 1.0678 - 1.0678 J/cm

@Thickness 3.17 - 3.17 mm
2.0004 - 2.0004 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.850 J/cm Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Izod Impact, Notched 1.0678 - 1.0678 J/cm

@Temperature -40.0 - -40.0 °C
2.0004 - 2.0004 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.07 J/cm Grade Count:9
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Izod Impact, Notched 1.0678 - 1.0678 J/cm

@Thickness 3.17 - 3.17 mm
2.0004 - 2.0004 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.07 J/cm Grade Count:9
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Izod Impact, Notched 1.0678 J/cm
2.0004 ft-lb/in
ASTM D256
Stratasys® ABS
ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur..