Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 - 1.87 J/cm | 2.20 - 3.50 ft-lb/in | Average value: 1.49 J/cm Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Izod Impact, Notched | 1.66 - 1.87 J/cm | 3.10 - 3.50 ft-lb/in | Average value: 1.77 J/cm Grade Count:3 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Izod Impact, Notched | 0.370 - 1.87 J/cm | 0.693 - 3.50 ft-lb/in | Average value: 0.799 J/cm Grade Count:19 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched | 0.534 - 1.87 J/cm | 1.00 - 3.50 ft-lb/in | Average value: 1.25 J/cm Grade Count:44 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.214 - 1.87 J/cm | 0.401 - 3.50 ft-lb/in | Average value: 0.968 J/cm Grade Count:124 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 1.33 - 1.87 J/cm | 2.50 - 3.50 ft-lb/in | ASTM D256 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Izod Impact, Notched | 0.883 - 1.87 J/cm | 1.65 - 3.50 ft-lb/in | Average value: 1.38 J/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Izod Impact, Notched | 0.534 - 1.87 J/cm | 1.00 - 3.50 ft-lb/in | Average value: 1.27 J/cm Grade Count:38 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Notched | 0.480 - 1.87 J/cm @Temperature -40.0 - 0.000 °C |
0.899 - 3.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.922 J/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.480 - 1.87 J/cm @Thickness 3.17 - 3.20 mm |
0.899 - 3.50 ft-lb/in @Thickness 0.125 - 0.126 in |
Average value: 0.922 J/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.267 - 1.87 J/cm | 0.500 - 3.50 ft-lb/in | Average value: 0.622 J/cm Grade Count:42 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |