Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.32034 - 1.00 J/cm @Temperature -40.0 - -40.0 °C |
0.60013 - 1.87 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.660 J/cm Grade Count:2 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.300 - 1.00 J/cm @Temperature -40.0 - -29.0 °C |
0.562 - 1.87 ft-lb/in @Temperature -40.0 - -20.2 °F |
Average value: 0.565 J/cm Grade Count:9 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 1.00 - 1.00 J/cm @Temperature 0.000 - 0.000 °C |
1.87 - 1.87 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.960 J/cm Grade Count:2 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 1.00 - 1.00 J/cm @Temperature 0.000 - 0.000 °C |
1.87 - 1.87 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.945 J/cm Grade Count:3 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched | 0.300 - 1.00 J/cm @Temperature -40.0 - 0.000 °C |
0.562 - 1.87 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.512 J/cm Grade Count:3 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Izod Impact, Notched | 0.430 - 1.00 J/cm | 0.806 - 1.87 ft-lb/in | Average value: 0.731 J/cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.800 - 1.00 J/cm | 1.50 - 1.87 ft-lb/in | ASTM D256 |
Loxim 120 01V0 Polycarbonate, 20% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.900 - 1.00 J/cm | 1.69 - 1.87 ft-lb/in | ASTM D256 |
Loxim 330 01V0 Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.800 - 1.00 J/cm | 1.50 - 1.87 ft-lb/in | ASTM D256 |
Loxim 811 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.800 - 1.00 J/cm | 1.50 - 1.87 ft-lb/in | ASTM D256 |
Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant Information provided by Loxim Industries |