Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.21 J/cm | 7.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® EX75 ABS Multi-purpose, extrusion ABS providing a favorable balance of engineering properties. |
|||
Izod Impact, Notched | 4.21 J/cm | 7.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF004AL is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Notched | 4.21 J/cm | 7.89 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer LNP* THERMOCOMP* KF004AL is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. Added features of this material include: Low Extractible. |